Hardness and colour trends along the 76 wt.% Au (18.2 carat) line of the Au-Cu-Al system
- Publication Type:
- Journal Article
- Citation:
- Scripta Materialia, 2002, 47 (2), pp. 95 - 100
- Issue Date:
- 2002-07-01
Open Access
Copyright Clearance Process
- Recently Added
- In Progress
- Open Access
This item is open access.
Colour and hardness were measured on a series of alloys along the 76 wt.% Au line of the Au-Cu-Al system. Complex, non-monotonic behaviour was observed, which is shown to be correlated with microstructural changes. The available colours include reddish, yellow, 'apricot', white and purple. The hardness of as-cast material varies from 150 to 500 Vickers. © 2002 Acta Materialia Inc. Published by Elsevier Science Ltd. All rights reserved.